OXIDATION NOT REQUIRED If you choose to oxidize the alloy raise the temperature of the furnace to 980 deg.C Hold the alloy at this temperature for 10 min. No vacuum required
PREPARATION FOR BONDING OPAQUE Use 50 - 110 aluminium oxide sand blasting. Clean with distilled water in an ultrasonic bath or with a steam cleaner